STEVEBR
Mechanical
- May 7, 2002
- 12
I recently Charpy V notch tested some 50Mn2 steel (CMn steel %C 0.47 - 0.55, % Mn 1.4 - 1.8 & % Si 0.17 - 0.37), in both the quenched and tempered and forged conditions. I have a Rp0.2 of 650 - 700N/mm² & Rm value of 900N/mm² & a % elongation value of between 16 - 20%. Values were taken at 20°C, -25°C & -40°C. Expecting to see charpy values in the region of 50J figures have been returned with values in the region of 10 - 20J.
Any ideas as to why the charpy values are so low?
Any ideas as to why the charpy values are so low?