Hello,
I have been reading through PD5500 to try and determine if there is a requirement to impact test the following material:
BS1501-224-490B-LT50
13mm thick dished end
The design temperature is -7degC to +70degC
I have been looking at Annex D Figure D.1 and it is unclear as the chart does not extend far enough.
Can anyone shed some light on this matter or point me in the right direction?
Cheers
Simon
I have been reading through PD5500 to try and determine if there is a requirement to impact test the following material:
BS1501-224-490B-LT50
13mm thick dished end
The design temperature is -7degC to +70degC
I have been looking at Annex D Figure D.1 and it is unclear as the chart does not extend far enough.
Can anyone shed some light on this matter or point me in the right direction?
Cheers
Simon