I am preparing drawings for charpy impact testing samples and have a question about what is the correct ASTM spec to call out for the plate.
The product to be shipped to the customer has 1" SA-312 316/316L pipe that is to be welded to SA-105 socket weld fittings, designed to ASME B31.3. The customer requests that we have impact tests done for the weld procedure to be used on these welds.
The charpy impact samples are to be cut from a plate that is to be made by welding a 3/8? thick section of 316 plate with another similar plate made from CS. I am having difficulty determining what plate specs are the correct ones to call out.
I've been looking in ASME B31.3 as well as 2008a Section II, part A but have yet to have a moment of clarity.
Any pointers will be much appreciated.
The product to be shipped to the customer has 1" SA-312 316/316L pipe that is to be welded to SA-105 socket weld fittings, designed to ASME B31.3. The customer requests that we have impact tests done for the weld procedure to be used on these welds.
The charpy impact samples are to be cut from a plate that is to be made by welding a 3/8? thick section of 316 plate with another similar plate made from CS. I am having difficulty determining what plate specs are the correct ones to call out.
I've been looking in ASME B31.3 as well as 2008a Section II, part A but have yet to have a moment of clarity.
Any pointers will be much appreciated.