I have to weld 2"sch80 A 312 TP 316L with A182 F316L Flange.The design code is ASME B31.3 & MDMT is -110 deg C. I got a PQR of P8 to P8 with Impact done at -196 deg C.The thickness of coupon was 7mm.
Fabrication drawing note shows Impact test is required per ASME B31.3 Now my question is, does my above PQR will support the above joint
Or 403.6 of ASME sec IX will come into play.
A quick reply is appreciated.
Fabrication drawing note shows Impact test is required per ASME B31.3 Now my question is, does my above PQR will support the above joint