The below query in reference to impact test specimen sizes as per ASME Section VIII Div. 1 (Clause UG-84(c)(2)(a)) & ASME Section VIII Div. 2 (Clause 3.11.7.2 (b)).

As per the above-mentioned clauses, is it mandatory to use impact test specimens of 10 mm x 6.7 mm if the absorbed energy is in excess of 240J (244J for Div. 2) for standard 10 mm x 10 mm size specimens?

Background
During impact testing of a welding procedure using SA 516 Gr. 70 base material, the impact test in HAZ was reported as 278J, 246J & 263J. The absorbed energy reported in the base material test certificates is in excess of 300J. Now the authorized inspector is insisting that it is mandatory to carry out retest using 10 mm x 6.7 mm specimens for both welding procedure and base material.
 
Replies continue below

Recommended for you

No, not mandatory for Div. 1....clause clearly states MAY be used...not SHALL be used.
 
Just one point to add, when sub-size specimens option is selected, lateral expansion in addition to absorbed impact energy shall also be reported. Fully agreed with David339933 that sub-size specimens are not mandatory for the subject scenario