14
I'm trying to find what pressure or energy would be required to indent copper by 1mm. To be more specific it would be for a piece of copper sheet that was about 1mm thick and resting on some dust like particles so nothing too hard underneath. It would be struck by a pin like object that had a rounded end of about 1mm diameter.

If anyone could help with what the best way to calculate this would be it would be much appreciated.

Thanks.
 
Replies continue below

Recommended for you

If you can specify the shape and the dimensions of the indenter you want to use, you might be able to set up a simple test with any hardness testing machine, setting the support as you wish.
Note that different tempers of copper may give different results.

 
This is a tough question to me. The result worths a paper.
 