Hi all,
As per Mill MTC (material: Low Alloy steel AISI 4140), it’s been noted that Mn, Cr & MO contents are slightly exceeding the maximum permissible limits as set in applicable standard ASME IIA (Table 2).
Test results in MTC - Mn: 1.10, Cr: 1.20 & Mo: 0.35
Max upper limit for AISI 4140 as per ASME II (Table 2): Mn: 1.00, Cr: 1.10 & Mo: 0.25
Can we accept this material? What is impact of Mn, Cr & Mo (if excess) on low alloy steel? Does it have any negative impact?
Regards
As per Mill MTC (material: Low Alloy steel AISI 4140), it’s been noted that Mn, Cr & MO contents are slightly exceeding the maximum permissible limits as set in applicable standard ASME IIA (Table 2).
Test results in MTC - Mn: 1.10, Cr: 1.20 & Mo: 0.35
Max upper limit for AISI 4140 as per ASME II (Table 2): Mn: 1.00, Cr: 1.10 & Mo: 0.25
Can we accept this material? What is impact of Mn, Cr & Mo (if excess) on low alloy steel? Does it have any negative impact?