Is IGC testing required for Alloy C-22 forging procured as per ASTM B564? If yes which method of ASTM G28 shall be used?

Regards,
Suraj
 
Replies continue below

Recommended for you

It is not a requirement, or supplementary requirement, of B564. Thus, it would have to be a purchaser's specified requirement. NACE Corrosion 2007, Paper 07202 has a good discussion regarding the use of, and acceptance criteria for, ASTM G28A and G28B with N06022.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 