Mn Si suggests a plain carbon steel (don't quote me on that though). As for stg... St is normally short for 'stahl' (steel) although the 'g' has me stumped.
Perhaps the 'g' might actually be a number... depending on the circumstances, could be a 6, 9 or even a 5. Still, struggling to make much meaning even out of that.
How old is the drawing?