I want to manufacture ASTM 860 GR WPHY 60 fittings. What ASTM pipe grade should be ordered as starting material?
 
Look at the API 5L X60 Pipe Grade.
 
Arkaprava Ghosh

Per ASTM A860 Wrought High-Strength Ferritic Steel Butt-Welding Fittings, Standard Specification ...

1. Scope*
1.1 This specification covers wrought high-strength ferritic
steel butt-welding fittings of seamless and electric fusion-
welded construction covered by the latest revisions of ASME
B16.9
and MSS-SP-75. Butt-welding fittings differing from
these ASME and MSS standards shall be furnished in accordance
with Supplementary Requirement S58 of Specification
A960/A960M
. These fittings are for use in high-pressure gas
and oil transmission and distribution systems.


ASME B16.9 Factory-Made Wrought Butt-welding Fittings

MSS SP-75 High-Strength, Wrought, Butt-Welding Fittings

ASTM A960 Common Requirements for Wrought Steel Piping Fittings, Standard Specification for

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
If you review the referenced ASTM specification, you will find there are limited chemical composition requirements but no reference to a particular grade of material with which to manufacture the fittings. The OP actually posed a good question related to starting material to manufacture fittings.

As I stated, a good starting material is API 5L Grade X60, which meets A 860 chemical composition and strength requirements to manufacture fittings. There are others starting materials as well.
 
Depends on how the material responds to the mandated heat treatment. Starting with a TMCP pipe and then heat treating it might lead to grief.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
The other option you have for starting material is A 105 for fittings. You would need to procure the pipe with chemical requirements listed in A 860.
 
Thankyou all. API 5l Gr X60 seems to be the best option.
 