I want to know the corrosive resistant material that can be case hardened up to 1mm

Status
Not open for further replies.

brahmaarya

Mechanical
Jul 28, 2015
2
Dear sir ,
We want to know the material that can be case hardened up to 1 mm but the material must be corrosion resistant
 
Replies continue below

Recommended for you

Not enough information. What is the application? Corrosion resistant to what environment?
 
If this is in reference to austenitic stainless steel, then try Bodycote's Kolsterizing or S3P processes.
 
Dear sir
this application is for ball and socket joint but it is to be used for open atmospheric conditions
 