Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

i need a method of statement for " CMC" or columns controls modulus

Status
Not open for further replies.

francois23

Geotechnical
May 13, 2009
3
i need a code or a method of statement for tthe columns controls modulus does anyone know a site?
 
Replies continue below

Recommended for you

CMC is a proprietary product, talk to their representatives in your state.
 
Basically a CMC is nothing else than a commercial name for rigid inclusions. Rigid inclusions are nothing else than piles, the difference being the design : you will allow your pile to settle 20 or more mm depending on allowable settlements for the structure above.
Method statements for construction are the same than for piles. For the design, each contractor has its method, generally based on finite elements models, but there is no code or standard.
 