looking for a good source for 309LCb or 309 NbL bare wire for submerged arc welding.
 
Replies continue below

Recommended for you

Thank You Sir

I was searching late last night and finally found Esab product line. I had forgotten about them because I haven't used their products in 15-20 years.

Again, thanks

My client thinks we can overlay CS with one (1) pass of this and attain t-347 chemistry, and that is all he wants to pay for. But he says if I don't reach desired results I will have to make another pass of t-347 at my cost. I think I will run my procedures and just build in another pass in my costs.

 