I can not find SA 36 for Saddle material in PV Elite 2017

Status
Not open for further replies.

miftahazhar

Mechanical
Nov 4, 2018
11
Hello. I have problem to select SA 36 for my saddle design in PV ELite 2017. Is PV Elite doesn't add SA 36 to the list of saddle material ? or SA 36 has different name in PV Elite 2017 ?

Thanks
 
Replies continue below

Recommended for you

There are some restrictions for SA-36. Do you meet all the conditions of UCS-6(b)?
 
There are no Sec VIII, Div 1 restrictions on the use of SA-36 for non-pressure parts, but miftahazhar, what IS your Code of construction, if any?

Have you contacted Intergraph? That is part of what you pay a license fee for.

Regards,

Mike



The problem with sloppy work is that the supply FAR EXCEEDS the demand
 