I wish to have a bracket made, the steel on the dwg is A588 but my vendor is asking to use Steel A572 Gr.C Type 2 instead.
The part to be made is a 1/4 thick right angle bracket with a couple of mounting flanges welded to it with 1/2" dia holes.
Application t support motor in open salty enviroment.
Need toselect steel for strength / durability and corrosion