Does anyone have a quick discription of a DIY generator for Hypochlorous Acid. Should be easy to make... A matter of electrolysis of salt water. Create a good, cheap really useful disinfectant for Covid 19, I understand... from reading, it's not snake oil.


Dik
 
It is the delivery method that is controversial.

[link ]Bill[/url]
--------------------
"Why not the best?"
Jimmy Carter
 
Do you know how to generate this?


Dik
 
This is how many pools are treated. The electrode structures are usually Ti.
And remember that they are trying to generate a couple of ppm.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Thanks... but any idea of how? a matter of an anode and cathode with a small DC voltage applied and a mild salt solution? Can I do this with a small battery pack? with the anode and cathode being titanium or something similar. Due to chloride ions, stainless steel would likely be inappropriate?

Dik
 
Maybe you can go to the website of several commercial products and see if collectively they give enough info to reverse engineer it.

Good Luck,
Latexman
Pats' Pub's Proprietor
 
Will try...

Dik
 
I found these links but something went wrong when I thought that I posted them.
Link
Link

[link ]Bill[/url]
--------------------
"Why not the best?"
Jimmy Carter
 
Thanks very much... good links.


Dik
 
Yes DC, these are both voltage and current controlled (I believe that V is primary).
In some of them they periodically reverse polarity to refresh the electrode.
Most that I have seen are all Ti.
There are some of these made using high alloy SS grades that work very well also.

If you want a stronger solution you need to look up they make bleach (they start by making pure Cl).


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
I understand for the HOCl, that you need a weak saline solution. I'm currently trying to dig up some titanium... and I don't want to remove the plates from my ankle... but, in a pinch...

Dik
 
Both salinity and pH matter, you get different species at different pH.As I recall you want slightly acidic (6.5-7) but I will look it up to check.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
If titanium is best, what is second best?

[link ]Bill[/url]
--------------------
"Why not the best?"
Jimmy Carter
 
3DDave: Thanks... very informative video.

EDStainless: thanks for the added info. Thinking of cobbling one of these cells together. Was planning to use regular DC charger 12-20 VDC, but it appears the USB voltage of 5 VDC seems to be OK. Also not sure how critical current is.

Dik
 
waross: I would think some form of duplex SS would work... many common SS metals do not work well with Chlorides.

Dik
 
In the comments on that video are discussions from people who do this process for a living and suggestions about what won't work well.
 
Thanks 3DD... I didn't look at the comments... will now do that...

Added: I'm about half way through the comments and some of them are better than the video... lots of technical stuff to look up.

Dik
 
There is a range of current density that you want.
This is fairly low voltage high current.
And slightly lower pH works a little better (under 6.5).
You can get away with some Ni alloys (C276, Monel 400) or some high alloy SS (AL-6XN).

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Don't know if it applies to what your are doing, but pool chlorinators use titanium plates with a coating of ruthenium oxide and/or iridium oxide. But they are not producing hypochlorous acid, as pool pH is too high for that.
 