May 6, 2003 #1 wpr Civil/Environmental Joined Nov 14, 2002 Messages 8 Location US Has anyone seen or had an instance where liquid hypochlorite and aqua ammonia are used to form chloramines? I've only used (or even seen) gas chlorine used with ammonia to form the chloramines (due to a high THM potential). Thanks
Has anyone seen or had an instance where liquid hypochlorite and aqua ammonia are used to form chloramines? I've only used (or even seen) gas chlorine used with ammonia to form the chloramines (due to a high THM potential). Thanks
May 8, 2003 #2 hydrae Mechanical Joined May 8, 2003 Messages 829 Location US Once the Chlorine is in the water it converts to hypochlorus acid and hypochlorite (according to pH) no mater if it was gas or bleach to start with. check out AWWARF document Optimizing Chloramine Treatment Number: 90620 BACKGROUND Chlorine http://www.awwarf.com/exsums/90620.htm This document is free to AWWARF members or for sale at the web site Upvote 0 Downvote
Once the Chlorine is in the water it converts to hypochlorus acid and hypochlorite (according to pH) no mater if it was gas or bleach to start with. check out AWWARF document Optimizing Chloramine Treatment Number: 90620 BACKGROUND Chlorine http://www.awwarf.com/exsums/90620.htm This document is free to AWWARF members or for sale at the web site