Hello
Please i would lika to simulate the mechanical behavior of a polyrethane material (stretsh can attain 120 of the initial lenght) so i used in the load a displacement U2 =120 and i used the hyperelastic material i have used tensile test data. But after i run the job i have not the same curve of tensile test strain is only equal to 2 can anyone help me?? thanks a lot
Please i would lika to simulate the mechanical behavior of a polyrethane material (stretsh can attain 120 of the initial lenght) so i used in the load a displacement U2 =120 and i used the hyperelastic material i have used tensile test data. But after i run the job i have not the same curve of tensile test strain is only equal to 2 can anyone help me?? thanks a lot