PaulTheMechGuy
Mechanical
I need to meet a 20 ppm max chloride content for water used for hydrotesting a pressure vessel we are manufacturing. The customers requirement says potable water is required. We've had the water coming into our plant tested and the chlorides are consistantly around 70 ppm. Does anyone else have this problem? Where do you get your water from to meet low chloride requirements? We have another job coming through requiring less than 2 ppm.