Hydrometer Problem combining ASTM D6913 and D7928

Pu73

Civil/Environmental
Joined
Mar 21, 2025
Messages
2
Im facing the issue of having a jump in the gradation curve when combining data from sieve analysis D6913 and hydrometer D7928
Basically the jump is up not down, which means if my passing #200 is 25%, the passing particle size 0.05mm is 30%. Which does not make sense.
Its organic soil and has a lot of small wood particles that can not be easily removed from the sample. I know this interfere with the accuracy of hydrometer results, but D7928 did not address this issue specifically.
The curve does not smoothen unless I went with SG=3 for example. Which does not make sense.
Any tips please?
 
Did you wash and shake the hydrometer specimen for the sieve test? If not, and you used two separate specimens as per the ASTM STPs, then it's possible that the hydrom specimen may have had a greater percentage of P200 than the shook gradation sample and this will cause an issue.
 
Did you wash and shake the hydrometer specimen for the sieve test? If not, and you used two separate specimens as per the ASTM STPs, then it's possible that the hydrom specimen may have had a greater percentage of P200 than the shook gradation sample and this will cause an issue.
Yes I did wash the hydrometer sample and shake it. I only use one sieve set per ASTM D7928 to avoid any calculation or lab mistakes, so the whole sample that I start with is washed and shaken together after the hydrometer is done. I'm sure nothing wrong was done regarding following the standard, it's just the unusual high amount of organics that is not possible to remove from the sample. I do not know if there is a way to mitigate that issue or some kind of calculation manipulation to make up for the high organic content, especially since I know exactly how much organics I have in my sample.
 
How much organic material is floating in your sedimentation cylinder during the test? Can you burn off the organics and perform the test on the resulting "duplicate" sample? Then, compare the gradation curves and see what it tells you.
 
Sodium hypochlorite bleach can also be effective at removing organics, if high temperature would damage the sample.
 