Has anyone experienced the development of hydrogen between the carrier pipe and the fully welded Type B steel repair sleeve? With enough hydrogen produced to dent the carrier pipe due to a thicker steel sleeve? Can an overdriven CP system produce hydrogen from the carrier pipe under a steel sleeve? Or because the steel pipe and steel sleeve are electrically connected, the CP acts on both equally.
Maybe same scenario as a blister within a pipeline wall. Or maybe not. Thanks, AWOL