Hello everybody:
In the Technical Specifications (for different plants) for gates of a hydroelectric plant, with respect to the seal plates and screws and lock nuts can be read:
Case a. Bolts for J seals: type 304 Stainless Steel, ASTM A 320.
Nuts for J seals: stainless steel A 194 (Armco Nitronic 60).
Case b. Seal plates and bolts: 304 stainless steel.
J seal keeper plate: 410 stainless steel.
Fasteners: Studs, Anchors, screws, nuts and Assembly Bolts: stainless steel.
Case c. Studs and bolts: martensitic stainless steel.
Washers and nuts: austenitic stainless steel.
Case d. Bolts: F593-304 (316).
Nuts: F594-304 (316).
Case e. Bolts: hot dip galvanized carbon steel.
Washers and nuts: stainless steel.
Any comment about the variety of these specs?
El que no puede andar, se sienta.
In the Technical Specifications (for different plants) for gates of a hydroelectric plant, with respect to the seal plates and screws and lock nuts can be read:
Case a. Bolts for J seals: type 304 Stainless Steel, ASTM A 320.
Nuts for J seals: stainless steel A 194 (Armco Nitronic 60).
Case b. Seal plates and bolts: 304 stainless steel.
J seal keeper plate: 410 stainless steel.
Fasteners: Studs, Anchors, screws, nuts and Assembly Bolts: stainless steel.
Case c. Studs and bolts: martensitic stainless steel.
Washers and nuts: austenitic stainless steel.
Case d. Bolts: F593-304 (316).
Nuts: F594-304 (316).
Case e. Bolts: hot dip galvanized carbon steel.
Washers and nuts: stainless steel.
Any comment about the variety of these specs?
El que no puede andar, se sienta.