I am looking for any suggestions regarding possible causes of cracking on a WC Co Cr coating that has been applied by HVOF.
The coating is ~ 0.006" thick and is applied to a 17/4 (H1150M condition)seal ring which is then pressure tested in an assembly. After pressure testing numerous radial cracks were observed throughout the complete circumference of the seal ring. These were confirmed using dye penetrant testing.
The seal ring design has been confirmed to be acceptable using FEA analysis and I am working on 2 possible root causes.
1/ Base material problem i.e. elastic limit has been exceeded
2/ Coating - wrong type
Any thoughts, ideas or previous experiences welcome
The coating is ~ 0.006" thick and is applied to a 17/4 (H1150M condition)seal ring which is then pressure tested in an assembly. After pressure testing numerous radial cracks were observed throughout the complete circumference of the seal ring. These were confirmed using dye penetrant testing.
The seal ring design has been confirmed to be acceptable using FEA analysis and I am working on 2 possible root causes.
1/ Base material problem i.e. elastic limit has been exceeded
2/ Coating - wrong type
Any thoughts, ideas or previous experiences welcome