The corner radius of Hollow Structural Sections (HSS) is not something that can be manipulated to order, and is part of the existing manufacturing paradigm of numerous HSS producers in North America. The typical outside corner radius of North American HSS is 2t, where t is the wall thickness of the as-produced HSS, to the standard ASTM A500-10.