Does anyone have a chart listing corner radius's for HHS rectangular tube steel?
Follow along with the video below to see how to install our site as a web app on your home screen.
Note: This feature may not be available in some browsers.
The corner radius of Hollow Structural Sections (HSS) is not something that can be manipulated to order, and is part of the existing manufacturing paradigm of numerous HSS producers in North America. The typical outside corner radius of North American HSS is 2t, where t is the wall thickness of the as-produced HSS, to the standard ASTM A500-10.