The circled connection on this HSS and the other connections in general --
I feel like these should just be everyday fillet welds, but I'm not sure and I was hoping for a second opinion, would a flare bevel be proper to use for the joist to tube weld, (I know I'm showing fillet). Also are there any checks that are special to HSS and these type of welded connections, I couldn't quite find anything in chapter K of 13th ed. that seemed to fit this circumstance besides the 'transverse loading perp. to HSS axis checks' ...
I'm grateful for any insight, thanks guys & gals!
Scott
Scott Shields
Ghafari Associates, LLC
I feel like these should just be everyday fillet welds, but I'm not sure and I was hoping for a second opinion, would a flare bevel be proper to use for the joist to tube weld, (I know I'm showing fillet). Also are there any checks that are special to HSS and these type of welded connections, I couldn't quite find anything in chapter K of 13th ed. that seemed to fit this circumstance besides the 'transverse loading perp. to HSS axis checks' ...
I'm grateful for any insight, thanks guys & gals!
Scott