Hello All,
I am a materials engineer and want to use HSLA-100 in one of our project.
would you please let me know how can I find HSLA100 manufactures?
OR
Is there anyone who has the data sheet of this alloy?

thank you in advance,
 
The Domex line of steels from SSAB are also worth a look.