In a jam. Existing 1.5" .135 t-23 welded to t-91 ( a stub) welded to heavy wall 2.25 cr upper header.

Every tube across panel. Forced outage.

Doing it by the book. Well versed in the specifics. Electrical resistance preheating is a huge production hog. Doing it on the header as well as the tube side.

I have read most of what's out there. All recommend er preheating.

The question:

If I keep heaters on the header... Can I propane pre heat the tube? Thinking adding tcs to the tube side, hand held propane, no flame on the tube, temp sticks.... All that.

Will it work?
 
Air propane torch preheating has often been used when welding tube to tube as you describe.
 
I agree with weldstand. Why would a T91 stub be used between a T23 and T22 header??? Makes no sense. Are you sure the header is not Gr 91??
 
^ Long story. We requested T-23. Unfortunately the T-23 we received was not of current code case and the AI booted it. We were also struggling to find T-23 tig wire. T-91 was the next best alternative.
 