Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to understand the symbol ellipsis " ..." in chemical composition table of ASTM

Status
Not open for further replies.

lslcpfcc

Mechanical
Joined
Jul 20, 2016
Messages
36
Location
JP
Dear, bro,
In ASTM material specification, each specification specifies the chemical composition of that material, shown as the fellow table,
1_pguc4h.jpg

2_xxmgm0.jpg


in some column, there is a symbol ellipsis " ..." in that line, the note of this table indicates: the ellipsis " ..." represents "no requirement"

How to understand "no requirement" ? Does it imply the chemical element that the symbol ellipsis " ..." appeared Cann't present in this material. in other words, it implies this chemical element can be included in the material.
 
Simply, it means that analysis for that element is not required to be reported on the MTR.
 
This has been asked on ET before by others and weldstan is correct.
 
Dear weldstan
As your point, that analysis result for that element is not required to be reported on the MTR. If the result of the element is very high or very low, how can the purchaser judge the acceptance of the Material.


Can you send the web-link of that thread.Dear metengr ?
 
Generally speaking, the specifications limit the total amount of other elements not required to be reported. From a purchasing standpoint you can always ask for these elements to be reported.
 
lslcpfcc,