Howdy all,

I'm trying to figure out how to callout this marking process, since nothing in AS478 seems to cover it. We want to mark a part using a laser to cure a coating onto stainless steel sheet. The process is to apply dry moly lube or a specialty product like CerMark and then cure the material using a ~60W CO2 laser similar to what Omtech makes. After cure the part is cleaned and the un-cured coating wipes away leaving a clear dark mark. For my limited testing the marking seems stable and solvent/skydrol resistant.

Thanks,

-Kirby
 
My experience...

AS478 Rev S... LASER marking ref 'is as good as it gets'.

MIL-STD-130N w/C1 Seems to have better definition for LASER marking.
 
Also run some samples. I don't recall laser marking coated parts.
Bare steel or Chem filmed aluminum.
Coated has been tag or rubber stamped.
Or engraved .but I think it will work.
 
A CO2 laser can't significantly etch stainless steel which is what I think the AS478 process is indicating which gives minimum/maximum limits for material removal. The process I'm using is more like fusing the coating onto the metal and everything else gets wiped away.

This is what it looks like:

S20250728_0009.jpg
 
A CO2 laser can't significantly etch stainless steel which is what I think the AS478 process is indicating which gives minimum/maximum limits for material removal. The process I'm using is more like fusing the coating onto the metal and everything else gets wiped away.

This is what it looks like:

View attachment 15920
It's good, very proffesional and visible
 
This is typically handled by an in-house specification for the process. Take the AS478 / MIL_STD-130 as a basis for selecting durability requirements and include any requirements for material cleaning and handling of the pre-cured material with regards to shelf life.

I would contact CerMark for their inputs on process requirements. They should have a motive to get included in AS478 and MIL-STD-130 as a recognized process.

Until then you will need to convince the end user that this is sufficiently permanent for the duty the item is subject to.
 
Following the lead on the last page of this doc from CerMark


Gets you to something like "apply laser bonded marking per NASA-HDBK-6003 para 5.1.5."

And this one gets you

NASA-STD 6002 NASA Marking Standard
- Section 5.3.1 Non-intrusive Marking Page 27

and MIL-STD 130M DOD Marking Standard, Table II

Once you know the term "laser bonding "you can also find a bunch of other suppliers, any of which might have further suggestions.
 