This pad flange should be fabricated as per JIS10K 450A dimension. It is used for connecting with agitator motor.

But I just found that bolt holes quantity is not correct (16 holes instead of 20 holes) :(

Now the only repair procedure to come up with is by plug welding all hole follow AWS D1.1 cause 5.26.5

Worst case is to cut off this flange and replace new one.

Is there any recommendation?

Thank you in advance.



 
Replies continue below

Recommended for you

I would expect it will cost less to replace it. Inspect the new one before installation.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Can you make an independent adaptor base using plate steel for the agitator with the correct hole pattern and a separate welded plate that has the incorrect hole pattern to the adaptor base?
 
thanks SnTMan & quadtracker

Now proceeding plug welding.

Agitator maker doesnt accept to add adaptor. this agitator is kinda special and already fabricated to conform with vessel dimension.
 
Well, good luck. Hope you don't have to tap into the weld metal.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 