i used a ppd antiozonant in sbr gaskets, but when the gasket it is installed on pvc pipe, this stain the surface. now i try to remove or blck the migration of the ppd to the gasket surface, any sugestion or method for this?
the best way that I find is put the gaskets in a oven at 150°C for 20 minutes and aply a talc.
the best way that I find is put the gaskets in a oven at 150°C for 20 minutes and aply a talc.