Hello,
This topic reminds me of a situation I ran into many years ago at a sheet metal vendor. I was pretty new and was sent to the vendor to perform some quality inspection before the parts were sent to our facility. The part in question was spec'd as 14ga steel. When I checked the part, I noticed it was 16ga steel. I brought it up to the fabricator and was told it was 14ga. I asked them to put calipers on the part and it measured around .062. They said that was correct. I said 14ga was .075. They pulled a piece of 14ga stock and I watched their guy measure the sample which measured .075. I pointed that out and then watched him squeeze the calipers so hard the measurement dropped to .062 and he said "see, it's .062". I told them to correct the part and left. Needless to say, we stopped using them and they were out of business in a short time afterward.
Kyle