MicSeven
Materials
- May 19, 2003
- 12
I have some rollers made by SKH 51 material. Could i use the electrochemical polishing technique to polish the surface of the SKH51 rollers?
SKH 51 (C:0.8~0.9, Cr:3.8~4.5, Mo:4.5~5.5, V:1.6~2.2, W:5.5~6.7)
SKH 51 (C:0.8~0.9, Cr:3.8~4.5, Mo:4.5~5.5, V:1.6~2.2, W:5.5~6.7)