Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How to polish scratched Sapphire crystal?

Status
Not open for further replies.

Bryex

Mechanical
Joined
Jun 24, 2001
Messages
23
Location
GB
Would it be possible to polish Corundum crystal with grinding wheel dust mixed with water to form a slurry. I know diamond slurry used when lapping is excellent at polishing SS to a mirror finish. So does anyone reckon the former method would be possible? I suppose it depends on the grit size.


Bry
 