Hi all-

We're trying to design a front-panel for a device that will be a single piece of plastic. We need to have a clear window in the middle (where an LCD display is placed), and the rest should be Near-IR transmissive (>800nm) and opaque to visible light.

Is there a way to make this as a single part?
Or, would this be a clear plastic part that is painted/coated with IR transmission material?

Any guidance would be helpful.


Sincerely,
Erez
 
An opaque plastic cannot be made transparent with a coating; it's already inherent in the bulk properties of the material. You could possibly coat the non-transmitting portions to block visible, however. Why do you need it transparent to NIR?

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529

Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
 
The device has some electrical components that are InfraRed (IR Emitters, IR CMOS Sensor, etc.). These need to be hidden from the user, that's why the Infrared transmission coating.

How would a transparent piece of plastic be covered? Do you know such Infrared transmission materials and how they would be applied only on a part of the plastic?
 