I am faced with a problem of using an aluminum pinion gear and a steel spur gear. This project is time sensative. In other words I have no time for Hard coating the aluminum gear.
Can anyone suggest how to prolong the life of the Aluminum gear.
These gears have a fair amount of torque on them and move at a relatively hi RPM. I can't give exact #'s to rpm and torque because I simply do not know.
As of now I can get somewhere around 12 minutes of use from the aluminum gear and need to extend life to 35 minutes at least.
I hope someone can give me some information to make this possible.
Thank you.
Can anyone suggest how to prolong the life of the Aluminum gear.
These gears have a fair amount of torque on them and move at a relatively hi RPM. I can't give exact #'s to rpm and torque because I simply do not know.
As of now I can get somewhere around 12 minutes of use from the aluminum gear and need to extend life to 35 minutes at least.
I hope someone can give me some information to make this possible.
Thank you.