How to find the Japanese standards on aluminum die casting alloys?

Status
Not open for further replies.

shanghai

Mechanical
Joined
Oct 22, 2000
Messages
3
Location
US
Hello everyone,
Could anybody tell me how to find the Japanese standards on aluminum die casting alloys:JIS H5302-76 (or90)on the Internet? I just want to know the phisical and mechanical properties of the aluminum alloy ADC12(named by JIS).

Thanks a lot,

Mike Gu (from Sauer-Danfoss)
My email address is: mgu@sauer-danfoss.com
 
Only chemical composition of ADC12 in JIS H 5302, 1.5 to 3.5%Cu, 9.6 to 12.0%Si, max. 0.3%Mg, max. 1.0%Zn, max. 1.3%Fe, max. 0.5%Mn, max. 0.5%Ni, max. 0.3%Sn, Al remains.
 
go to metalinfo.com. they have this standard in their database. It is a paid membership service but have a free trial for a day.
 