How to determine whether metal is 316 or 316L? 1

Status
Not open for further replies.

jasgeer

Materials
Feb 22, 2002
7
We have a XRF alloy analyzer, but it is insenstive to carbon. Is there a simple test to measure carbon content that we can run to determine if a material is 316 vs 316L, or 304 vs 304L? We need to identify metals at incoming inspection and on our shop floor.
Thanks for your ideas!
 
Replies continue below

Recommended for you

For this level of material identification, you need a quantitative chemical analysis to determine carbon content. You have two options;

- either send out a small sample of each shipment of material that is received in your shop to a metallurgical lab for chemical analysis OR
- consider purchasing a desktop emission spectrometer for your company. There are web sites that advertise these devices including the example shown below;


If your volume of testing is sufficient, it may be worthwhile to investigate purchasing this device.
 