Hi,
How do I determine if I required the Expansion Joint for shell and Tube heat exchanger(fixed Tubesheet type)?
Following are the max temperature for each condition listed below.
Design Conditions
Shell side P(psig)=150 Temp(min/Max)=32/250 deg F
Tube side: P(psig)=150/FV Temp9min/Max)=32/250 deg F
Shell Shell Tube Tube
sideT side P sideT side P
(F) (psig) (F) (psig)
Normal Operation 43 50 57 -15
"Shell side fluid on
-Tube side fluid off" 32 57 32 0
"Tube side fluid on
-Shell side fluid off" 70 0 142 -15
Steam Out condition 70 0 278 25
MOC is:
Shell= carbon steel(SA106B)
Tube= Hastelloy B3(SB626 UNS N10676)
Thanks for your response!!
Mechmania
How do I determine if I required the Expansion Joint for shell and Tube heat exchanger(fixed Tubesheet type)?
Following are the max temperature for each condition listed below.
Design Conditions
Shell side P(psig)=150 Temp(min/Max)=32/250 deg F
Tube side: P(psig)=150/FV Temp9min/Max)=32/250 deg F
Shell Shell Tube Tube
sideT side P sideT side P
(F) (psig) (F) (psig)
Normal Operation 43 50 57 -15
"Shell side fluid on
-Tube side fluid off" 32 57 32 0
"Tube side fluid on
-Shell side fluid off" 70 0 142 -15
Steam Out condition 70 0 278 25
MOC is:
Shell= carbon steel(SA106B)
Tube= Hastelloy B3(SB626 UNS N10676)
Thanks for your response!!