The flue gas from our CDU(Crude distillation unit) heater is heat exchanged with the heater inlet air.
The air preheater is a static type with cast iron fin tube in the upper section and glass tube in the lower section.
There is a DeNOx facility(SCR) upstream of the air preheater.
We encounter serious plugging problem in the upper section of the air preheater.
How to clean the air preheater? By water jet? or
Do we need to dismantle the air preheater?
The air preheater is a static type with cast iron fin tube in the upper section and glass tube in the lower section.
There is a DeNOx facility(SCR) upstream of the air preheater.
We encounter serious plugging problem in the upper section of the air preheater.
How to clean the air preheater? By water jet? or
Do we need to dismantle the air preheater?