May 25, 2002 #1 psozot Electrical Joined Apr 15, 2001 Messages 45 Location PK can someone tell me how to calculate weight of MS pipe.i am in need of thumbrule for calculating things like "cost/inch/meter"
can someone tell me how to calculate weight of MS pipe.i am in need of thumbrule for calculating things like "cost/inch/meter"
May 27, 2002 1 #2 MortenA Chemical Joined Aug 20, 2001 Messages 2,998 Location DK If you use a standard schedule then usually this will also list weight/m (ft whatever). If you dont, simply multiply wall thickness with OD and lenght and density of steel (around 7900 kg/m3) and there you have it. Upvote 0 Downvote
If you use a standard schedule then usually this will also list weight/m (ft whatever). If you dont, simply multiply wall thickness with OD and lenght and density of steel (around 7900 kg/m3) and there you have it.