The tangent Modulus is just that - the tangent of the stress-strain curve at any particular point. If you have a stress-strain curve, then you can calculate the tangent modulus either symbolically, if you have a formula (derivatives, calculus-type stuff), or numerically (delta stress / delta strain).
Don't over-think this. Draw the stress-strain curve out. draw your tangent modulus lines. Should be easy...