Load testing is one way, but there is an easier way, namely to calculate the properties and determine the allowable load from that. You need to know the grade of steel, specifically the value of E and Fy.
In Canada, you would check against CSA S-136 the code for Cold Formed Structural Members. The effective width may be smaller than the total width for light gauge material. A different code may apply in your area.
BA