Tmoose
Mechanical
- Apr 12, 2003
- 5,636
On another forum a discussion about storing performance summer tires has sprung up. One theory offered is that new Englanders should keep their cherished summer tires in the living room for the winter, fearing that deep cold cycles (not cryogenic) would change the sticky rubber's structure to the worse.
Is there any thing to fear (or prefer) leaving the tires in an unheated garage?
thanks
Dan T
Is there any thing to fear (or prefer) leaving the tires in an unheated garage?
thanks
Dan T