how much temperature for stainless steal during welding
 
Replies continue below

Recommended for you

It depends on the alloy, some have very strict (low) interpass temperatures.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
That is like asking what is the temperature of water. It depends. More information please. Material grade, application, code of construction???
 
What are you asking for? The melting point range of standard alloys? The temperature of the molten puddle of the weld metal being deposited? What welding process?
 