Jun 5, 2003 #1 BRT549 Chemical Joined Dec 27, 2002 Messages 115 Location US Looking for a weight, but don't have a handy reference. It's a 36" size.
Jun 5, 2003 1 #2 TangoCleveland Mechanical Joined Jun 28, 2002 Messages 224 Location US 1676 lb. Check http://www.texasflange.com/catalog.pdf Larry Upvote 0 Downvote
Jun 5, 2003 #3 Shubijj Industrial Joined Apr 9, 2003 Messages 2 Location MX There are other reference: "Grinell pipe hanger design and engineering / weights of piping materials", the weight marked there is 1233 Lbs. Regards. Shubijj. Upvote 0 Downvote
There are other reference: "Grinell pipe hanger design and engineering / weights of piping materials", the weight marked there is 1233 Lbs. Regards. Shubijj.
Jun 5, 2003 Thread starter #4 BRT549 Chemical Joined Dec 27, 2002 Messages 115 Location US Thanks, OldSohioEngr - the link was exactly what I was looking for. All my handbooks only went up to 24". Upvote 0 Downvote
Thanks, OldSohioEngr - the link was exactly what I was looking for. All my handbooks only went up to 24".