Hi,
My question seems to be "simple" but I can not find an answer.
The specification of our costumer in a steel alloy composition is :
0.55 Cr % Max
But our chemical analysis shows the value of 0.552 % of chromium.
• . If we around the value of 0.552 to 0.55 we met the requirements.
• . If we dont around the value of 0.552 we don't met the requirements.
• Specific question: what is the right thing to do in this case ?
• General question : how many digits must be required in the chemical composition specifications ?
Thanks in advance ?
My question seems to be "simple" but I can not find an answer.
The specification of our costumer in a steel alloy composition is :
0.55 Cr % Max
But our chemical analysis shows the value of 0.552 % of chromium.
• . If we around the value of 0.552 to 0.55 we met the requirements.
• . If we dont around the value of 0.552 we don't met the requirements.
• Specific question: what is the right thing to do in this case ?
• General question : how many digits must be required in the chemical composition specifications ?
Thanks in advance ?