Similar format charts to those posted by TD2K, but looks like the time to first maintenance is a lot longer. It depends a lot on the thickness of the base metal, as the thicker the steel, the more zinc.
The thickness of zinc deposited should be part of the spec sent to the fabricator / galvanizer, usually in ounces per square foot, or in Grades per ASTM A123, sometime in mils.