I have a project in Southern California where I have an existing 8" transite water pipe that I plan on tapping into for a new 3" domestic water service lateral. My 3" pipe will be Type K copper. I am looking for the least expensive way to connect the two pipes. The easiest would be a 3" service saddle. Most cities, if not all here, allow only 2" and below. This is on a private site so city has no jurisdiction but I'm sure there is a reason for keeping it below 2". Smith-Blair makes a 3" service saddle, but is this the best way to go? I could also consturct an 8" x 3" tapping sleeve (stainless steel or ductile iron) but how do I connect my 3" copper pipe so electrolysis does not occur? Help!!